Cell design

The lithium balance: designing a cell forwards

Five short parts on how anode, cathode and lithium are designed against each other, how they age, and what happens when you blend materials. Equilibrium only, tanks and straight lines, and a small tool in every part.

5 · Two tanks, one level: blended electrodes

So far every electrode had exactly one material. In reality that's less and less the case: in almost every high-performance cell today, the anode has some silicon blended in. How does that fit into the tank picture?

Two tanks, one pipe

Picture a blended anode as two different tanks, connected at the bottom by a pipe. So the level is always the same in both, because both materials sit at the same potential.

Before you read on: when you charge a silicon–graphite anode, which material takes up lithium first?

Remember the ceiling? That's what we measure every material against. Silicon starts taking up lithium much earlier, so its tank hangs lower, further away from the ceiling. The graphite tank hangs higher.

Two linear tanks connected at the bottom. The silicon tank hangs lower, so it fills first.

On charge, at first only the silicon tank fills, until the level reaches the bottom of the graphite tank. From then on both fill together: two tanks share the water, the level rises more slowly, and right there the voltage curve has a kink.

25
0.50
The connected tanks
Potential of the blend
Where the lithium goes
Potential vs Li/Li⁺
–
Lithium in silicon
–
Lithium in graphite
–

Graphite and silicon

Graphite takes up lithium in clear steps, hence the plateaus. Silicon takes it up more continuously, so its tank is a bit slimmer.

Connect the two and the sharp kink becomes a smooth transition, and graphite and silicon share the lithium depending on where the level is.

If you know dQ/dV: that's exactly the width of the tanks. With real curves, graphite shows sharp peaks and silicon a broad hump; linear tanks give two boxes. In the blend, the graphite peaks simply sit on top of the silicon hump. And because the widths simply add up, you can turn it around: from a measured dQ/dV curve you can read off how much graphite and how much silicon contribute.

70
Top: the blend and your graphite. Bottom: what's left for silicon (own scale).
Graphite share (guess)
–
Remainder
–

On the cathode side it works the same way, for example NMC with LFP.

The math behind it

qiq_i lithium in material ii, QiQ_i its tank size, Ui0U_i^0 its empty tank, sis_i its slope, gg dQ/dV, ww graphite share.

Each tank

U=Ui0−si qisi=ΔUiQiqi(U)=Ui0−Usi\begin{aligned} U &= U_i^0 - s_i\,q_i \\[4pt] s_i &= \frac{\Delta U_i}{Q_i} \\[4pt] q_i(U) &= \frac{U_i^0 - U}{s_i} \end{aligned} 0≤qi≤Qi0 \le q_i \le Q_i

Blend at one potential

q(U)=∑iqi(U)q(U) = \sum_i q_i(U)

Slope after the kink

1s=1sGr+1sSi\frac{1}{s} = \frac{1}{s_\mathrm{Gr}} + \frac{1}{s_\mathrm{Si}}

dQ/dV of the blend

gblend=w gGr+(1−w) gSig_\mathrm{blend} = w\,g_\mathrm{Gr} + (1 - w)\,g_\mathrm{Si}

Questions, or a cell where this doesn't fit? Write me or find me on LinkedIn. The full models with real material curves are on the tools page.