Why cells get thicker
A silicon/NMC stack breathes with the state of charge, grows with its SEI and pushes back when you clamp it.
What makes a cell thicker
- Breathing: both electrodes change volume with the state of charge, the silicon anode most of all. The SoC slider drives it.
- SEI growth: the SEI keeps growing over life and adds thickness that never goes away. The lower the SoH, the thicker the stack.
- Compression: clamp a pouch or prismatic cell and you squeeze the pores: the stack gets thinner, the porosity drops. A cylindrical can fixes the thickness instead.
Model settings
The cell pairs a silicon anode with an NMC cathode (N/P 1.1, Li/P 0.95, 2.8 to 4.2 V). The stack consists of the anode current collector (18 µm), anode (7 µm), separator (20 µm), cathode (47 µm) and cathode current collector (15 µm), with porosities of 0.3 (anode), 0.4 (separator) and 0.25 (cathode). Thicknesses are normalised to the designed stack: half of each current collector, both coatings and the separator.