Materials: what the shape of a tank tells you
LFP: what hides behind the flat line
More than half of the batteries going into new electric cars are now LFP. It's cheaper, it's safer, and it's notorious for giving modellers headaches, because it behaves so differently from most other materials here.
- Potential vs Li/Li⁺
- –
- Lithium in the material
- –
Over almost the whole capacity, the voltage sits at about 3.4 V. In the tank, that's one huge reservoir: the level stands still while the water keeps running in. Its width is not to scale: on a truly flat line, it would run off to infinity.
Where that flat line comes from only makes sense on two levels: one particle, and the millions of particles in an electrode. You need both.
Level 1: one particle
LFP is only comfortable in two states: almost empty (FePO₄) and almost full (LiFePO₄). Each, on its own, is an ordinary narrow tank: only over the first and the last few percent does extra lithium actually raise the level.
Now fill a particle evenly beyond that, and it gets strange. The voltage first dips below the flat line, then climbs back above it while you keep adding lithium, which is the wrong way round. The curve of one evenly filled particle isn't flat at all: it's an S. On its middle stretch, the particle is unstable and won't stay there.
So it splits. Take a typical LFP particle, a thin platelet. At first, the whole platelet takes up lithium evenly and gets a little bluer. Then, all of a sudden, it splits into a lithium-rich and a lithium-poor phase, side by side at the same level, and from there only the boundary between the two moves. Phase-field models follow exactly that; Bazant and co-workers have done a lot of it, and I've had my fair share too.
Let's look at what the curve does meanwhile. At first, it follows the S exactly and dips below the flat line. When the particle splits, it suddenly snaps back up and stays flat until the very end, when all the FePO₄ has turned into LiFePO₄. In a real cell, we don't see this snap. To understand why, we need to go one level up: to the particle population.
Before you read on: an LFP electrode rests at 50 % state of charge. What do its particles look like?
Almost every particle is either full or empty; only a few are on their way. The 50 % isn't inside the particles, it's how many of them have already tipped over.
Level 2: the population
The answer is the crowd. An electrode holds millions of particles, each with its own push to overcome. At the edges, they all fill together. On the plateau, one particle tips over and converts completely while the others wait, then the next one, and the next. The waiting ones sit just before their split, at the bottom of the dip, and they hold the voltage there. So the electrode never snaps back.
The states in between no longer sit inside a particle; they're in the electrode: some particles full, some still empty. In the tank, that's the weir: two narrow tanks, one for the empty and one for the full state, and in between a reservoir at one height. The reservoir is the share of particles that have tipped over, and for the population, it's stable. Dreyer and co-workers worked out this population picture for LFP. How many particles tip at once depends on the current: slowly, one after another; fast, many at the same time (Li et al.).
And that's the link back to the flat line you measure. It isn't in either of the two states, and not in a single particle either: that one snaps. It appears in how the population fills, one particle after another: an emergent property. What the material does fix is the height of the crest, the one level at which both states are equally happy.
On the way back, it runs the same way, just in reverse: one particle after another turns from LiFePO₄ back into FePO₄. And again, each one needs its own push, this time from the other side. That's why the level depends on the direction: just above the crest on the way in, just below it on the way out, however slowly you go. That's the hysteresis: the voltage sits a little higher when you charge the cell than when you discharge it.
For the curious: where the S comes from
Some materials undergo phase changes, and we can trace this back to a single interaction term that says how well neighbouring lithium ions get along. This is called a regular solution. Turn the knob:
- Shape
- –
To the left, the ions push each other away, and the tank gets narrow and tall. In the middle, you're back at the ideal bell. To the right, the bell gets wider and flatter. Now watch the free energy: below 2 kT it has a single minimum, and the crystal fills evenly. Above 2 kT it turns into a double well. Every filling between the two minima is cheaper as a mix of a lithium-poor and a lithium-rich phase than as one evenly filled crystal, so the material splits. In the tank, the middle becomes a reservoir at one height. That's the weir from above, and it's where plateaus come from.
free energy per site, chemical potential of lithium (the voltage is ), interaction between neighbours (here in units of , positive = they attract).
Regular solution: entropy plus one interaction term
When the double well appears
Then the two phases sit where one common tangent touches both minima. Between them, the potential is flat: the plateau.
LFP sits far to the right on that knob, at about 4.5 kT. Fill it evenly, and its voltage comes out as an S. In the middle of the S, more lithium raises the voltage. But lithium always moves towards the higher voltage. So a spot that happens to hold a little more lithium pulls in more from its neighbours and gets richer still, and the crystal splits by itself. That's spinodal decomposition. The two phases then sit side by side at one potential, the plateau. It cuts the S so that the areas above and below are equal (Maxwell's construction).
On the shelf, LFP sits in the middle, a good bit higher than NMC. Against graphite, the waterfall is shorter, so the cell has less voltage. In return, the material is extremely stable: both of its states are stable compounds, and the phosphate holds on tightly to its oxygen.
Sources for this part
- Curves: half-cell measurement (Canrd), LiFePO4 type D-3, 0.1C, first cycle, digitised (see Data source at the bottom). Not an open-circuit voltage: part of the gap between the two curves is overpotential, not hysteresis. Weir, particles and S-curve are sketches.
- IEA, Global EV Outlook 2026: LFP above 55 % of the EV batteries deployed in 2025.
- Dreyer, Jamnik, Guhlke, Huth, Moškon and Gaberšček, The thermodynamic origin of hysteresis in insertion batteries, Nature Materials 9 (2010) 448, doi:10.1038/nmat2730: many particles, each either empty or full, and the hysteresis at zero current.
- Bai, Cogswell and Bazant, Suppression of phase separation in LiFePO4 nanoparticles during battery discharge, Nano Letters 11 (2011) 4890, doi:10.1021/nl202764f: phase separation inside one particle, and how current suppresses it.
- Li et al., Current-induced transition from particle-by-particle to concurrent intercalation in phase-separating battery electrodes, Nature Materials 13 (2014) 1149, doi:10.1038/nmat4084: one by one at low rates, many at once at high rates.
- Castelli, von Kolzenberg, Horstmann, Latz and Dörfler, Efficient simulation of chemical–mechanical coupling in battery active particles, Energy Technology 9 (2021) 2000835, doi:10.1002/ente.202000835: phase field with mechanics, inside LFP particles.
Data source
All curves in this chapter except graphite and silicon are half-cell measurements by Canrd, published with their materials and used here with their kind permission.