Materials: what the shape of a tank tells you
NMC/NCA: the same tank, emptied further
NMC is the cathode for anything where range counts: a layered oxide, in which lithium sits in thin sheets between layers of metal and oxygen.
- Potential vs Li/Li⁺
- –
- Lithium in the material
- –
- Used between 3.0 and 4.3 V
- –
The name is the formula: lithium nickel manganese cobalt oxide, LiNixMnyCozO2 with x + y + z = 1; NMC811 means 8 : 1 : 1. And the formula already gives away two things.
Before you read on: which one has the highest theoretical capacity?
First, the size of the tank. There's one lithium per formula unit, and nickel, manganese and cobalt weigh almost the same. So every NMC carries one lithium per roughly 97 g of material, about 275 mAh/g, whatever the mix. All NMC tanks are the same size, at least in theory.
Second, the price. Per kilogram, cobalt costs several times as much as nickel, and manganese is cheap. So the more cobalt, the pricier the NMC, and that's why cobalt keeps getting pushed out: from NMC111 via 622 to 811 and beyond.
What the mix does change is how far you can empty the tank. More nickel pulls the curve down, so at the same upper limit you get further into the tank. So nickel is the knob that matters: more of it means less cobalt and more of the same tank in use. What you pay for it is stability: the more nickel, the more reactive the charged material. It's a game of filling levels, not tank size.
Why are there no steps?
Up to NMC622, the curve falls evenly and smoothly. Lithium spreads evenly through the whole material, so every bit of it raises the level a little: the tank is narrow, tall and roughly the same width all the way down, without a reservoir. From NMC811 onwards, a small step shows up near 4.2 V; more on that below.
NMC has a close cousin, NCA, with aluminium instead of manganese. It behaves very similarly, and the more nickel you put into either, the closer both get to the same material: lithium nickel oxide.
NMC sits at the bottom of the shelf, far below the ceiling. That distance is the high cell voltage you get against graphite. The catch: the more lithium you pull out, the emptier the framework that holds it, and at some point the structure starts to suffer. More nickel brings capacity, but it also takes you closer to that limit.
From NMC811 on, you can see it in the tank: a small reservoir near 4.2 V, where the layers suddenly pull closer together (the H2→H3 transition). That sudden shrinking strains the particles until they crack, and it's one of the main reasons high-nickel cells aren't charged much further. So why not just charge higher anyway? That's exactly what LCO does.
Sources for this part
- Curves: half-cell measurements (Canrd), 0.1C, first discharge between 3.0 and 4.3 V (NCA 4.25 V), digitised (see Data source at the bottom). Not open-circuit voltages: the overpotential is still in them. Dashed above the cut-off: extrapolated as a solid-solution tail up to 4.6 V, not measured. Where Canrd offers several products of one composition, the curve is the one in the middle.
Data source
All curves in this chapter except graphite and silicon are half-cell measurements by Canrd, published with their materials and used here with their kind permission.